Calspar N

Description: Sodium feldspar

Oxide Analysis Formula Tolerance
CaO 0.49% 0.07
K2O 0.29% 0.02
MgO 0.12% 0.02
Na2O 7.10% 0.89
Al2O3 13.76% 1.04
SiO2 77.48% 9.97
Fe2O3 0.22% 0.01
LOI 0.54%n/a
Oxide Weight 769.18
Formula Weight 773.35