| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.13% | 0.01 | |
| K2O | 4.95% | 0.31 | |
| MgO | 0.35% | 0.05 | |
| Na2O | 0.40% | 0.04 | |
| TiO2 | 0.15% | 0.01 | |
| Al2O3 | 17.38% | 1.00 | |
| P2O5 | 0.03% | - | |
| SiO2 | 69.02% | 6.74 | |
| Fe2O3 | 2.97% | 0.11 | |
| MnO | 0.02% | - | |
| LOI | 4.60% | n/a | |
| Oxide Weight | 559.88 | ||
| Formula Weight | 586.88 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |