| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| K2O | 6.40% | 0.23 | |
| Na2O | 0.30% | 0.02 | |
| Al2O3 | 29.80% | 1.00 | |
| P2O5 | 0.01% | - | |
| SiO2 | 55.50% | 3.16 | |
| Fe2O3 | 0.40% | 0.01 | |
| LOI | 8.10% | n/a | |
| Oxide Weight | 316.99 | ||
| Formula Weight | 344.93 | ||