| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.12% | 0.01 | |
| K2O | 10.16% | 0.73 | |
| MgO | 0.07% | 0.01 | |
| Na2O | 2.23% | 0.24 | |
| Al2O3 | 21.31% | 1.41 | |
| SiO2 | 62.66% | 7.06 | |
| Fe2O3 | 0.25% | 0.01 | |
| LOI | 3.20% | n/a | |
| Oxide Weight | 655.39 | ||
| Formula Weight | 677.05 | ||