Stone B

Oxide Analysis Formula Tolerance
CaO 0.07% 0.01
K2O 5.44% 0.23
MgO 0.25% 0.02
Na2O 0.23% 0.01
TiO2 0.13% 0.01
Al2O3 25.35% 1.00
SiO2 63.24% 4.23
Fe2O3 0.27% 0.01
LOI 4.55%n/a
Oxide Weight 382.17
Formula Weight 400.39