| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.18% | 0.01 | |
| K2O | 4.81% | 0.19 | |
| MgO | 0.20% | 0.02 | |
| Na2O | 0.13% | 0.01 | |
| TiO2 | 0.13% | 0.01 | |
| Al2O3 | 28.11% | 1.00 | |
| SiO2 | 62.40% | 3.77 | |
| Fe2O3 | 0.21% | - | |
| LOI | 4.65% | n/a | |
| Oxide Weight | 348.96 | ||
| Formula Weight | 365.98 | ||