Silica Volatilized D

Description: SILICA

Oxide Analysis Formula Tolerance
CaO 0.02% -
K2O 0.05% -
MgO 0.02% -
Na2O 0.50% 0.05
TiO2 0.01% -
Al2O3 17.00% 1.00
0.02% -
P2O5 0.05% -
SiO2 82.00% 8.19
Fe2O3 0.10% -
Oxide Weight 598.50
Formula Weight 598.50

Notes

pH: 5-6
Pour Density (kg/m3): 250
Surface Area (m2/g): 15
Particle Size Distribution (D50): 0.5

A low pH, higher Al2O3 variety (Z) is also avalable.

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy