| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.11% | 0.01 | |
| K2O | 2.06% | 0.12 | |
| MgO | 0.79% | 0.11 | |
| Na2O | 1.00% | 0.09 | |
| Al2O3 | 18.03% | 1.00 | |
| SiO2 | 70.00% | 6.59 | |
| Fe2O3 | 1.75% | 0.06 | |
| LOI | 6.26% | n/a | |
| Oxide Weight | 530.31 | ||
| Formula Weight | 565.72 | ||