| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.04% | 0.10 | |
| K2O | 0.04% | 0.06 | |
| Na2O | 0.01% | 0.02 | |
| TiO2 | 0.56% | 0.99 | |
| Al2O3 | 0.72% | 1.00 | |
| SiO2 | 98.20% | 231.48 | |
| Fe2O3 | 0.30% | 0.27 | |
| LOI | 0.13% | n/a | |
| Oxide Weight | 14,148.25 | ||
| Formula Weight | 14,166.67 | ||