| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.02 | |
| K2O | 0.70% | 0.03 | |
| MgO | 0.40% | 0.04 | |
| Na2O | 0.10% | 0.01 | |
| TiO2 | 1.60% | 0.08 | |
| Al2O3 | 27.20% | 1.00 | |
| SiO2 | 58.10% | 3.63 | |
| Fe2O3 | 1.01% | 0.02 | |
| LOI | 10.60% | n/a | |
| Oxide Weight | 335.29 | ||
| Formula Weight | 375.04 | ||
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |