Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Nangoo Feldspar

Oxide Analysis Formula Tolerance
CaO 0.36% 0.05
K2O 3.47% 0.30
MgO 0.05% 0.01
Na2O 4.84% 0.64
TiO2 0.10% 0.01
Al2O3 14.47% 1.16
P2O5 0.01% -
SiO2 75.40% 10.23
Fe2O3 0.56% 0.03
MnO 0.01% -
LOI 0.73%n/a
Oxide Weight 809.51
Formula Weight 815.47

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy