| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.28% | 0.03 | |
| K2O | 3.30% | 0.22 | |
| MgO | 0.60% | 0.09 | |
| Na2O | 1.97% | 0.20 | |
| TiO2 | 0.05% | - | |
| Al2O3 | 16.03% | 1.00 | |
| SiO2 | 75.14% | 7.96 | |
| Fe2O3 | 0.42% | 0.02 | |
| LOI | 2.21% | n/a | |
| Oxide Weight | 622.24 | ||
| Formula Weight | 636.31 | ||