4-C Clay

Alternate Names: Spinks 4-C, 4-C Ball Clay

Oxide Analysis Formula Tolerance
CaO 0.26% 0.02
K2O 0.51% 0.02
MgO 0.22% 0.02
Na2O 0.16% 0.01
TiO2 1.27% 0.06
Al2O3 25.29% 1.00
P2O5 0.12% -
SiO2 58.64% 3.94
Fe2O3 1.26% 0.03
LOI 12.28%n/a
Oxide Weight 353.83
Formula Weight 403.37

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

Data

Pyrometric Cone Equivalent 31.5
Dry M.O.R. (50% Silica) 437C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy