WL Rhyolite

Alternate Names: WL Rhyolite (Hanks)

Description: From Ron Roy\'s MDT

Oxide Analysis Formula Tolerance
CaO 1.16% 0.16
MgO 0.50% 0.10
K2O 4.90% 0.40
Na2O 2.80% 0.35
TiO2 0.20% 0.02
Al2O3 11.60% 0.87
SiO2 76.20% 9.73
Fe2O3 2.60% 0.12
Oxide Weight 767.37
Formula Weight 767.37

Related Information

Links

URLs http://en.wikipedia.org/wiki/Rhyolite
Rhyolite at Wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy