Description: A sodium aluminum silicate with chlorine
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 31.00% | 0.75 | |
| Na2O | 25.00% | 1.00 | |
| SiO2 | 37.00% | 1.53 | |
| Cl | 7.00% | n/a | |
| Oxide Weight | 230.64 | ||
| Formula Weight | 248.00 | ||
| Minerals |
Sodalite
A sodium aluminum silicate with chlorine |