Description: High iron mineral
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 7.80% | 0.44 | |
| Al2O3 | 8.40% | 0.28 | |
| Fe2O3 | 1.70% | 0.04 | |
| FeO | 35.60% | 1.47 | |
| MnO | 0.40% | 0.02 | |
| MgO | 4.00% | 0.34 | |
| CaO | 10.50% | 0.63 | |
| TiO2 | 0.20% | 0.01 | |
| P2O5 | 1.30% | 0.03 | |
| H2O | 4.20% | n/a | |
| CO2 | 25.30% | n/a | |
| Oxide Weight | 236.48 | ||
| Formula Weight | 335.44 | ||