| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.05% | - | |
| K2O | 0.80% | 0.01 | |
| MgO | 0.15% | 0.01 | |
| Na2O | 0.30% | 0.01 | |
| TiO2 | 0.20% | - | |
| Al2O3 | 73.30% | 1.00 | |
| SiO2 | 24.70% | 0.57 | |
| Fe2O3 | 0.50% | - | |
| Oxide Weight | 139.15 | ||
| Formula Weight | 139.15 | ||
Particle Size: 1.5-3.0mm
Free iron grains: .02% max
Grain porosity: 3%
Bulk density: 2.89 g/cm3
Refractoriness: 1875/1900C
| Typecodes |
Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes. |
| Density (Specific Gravity) | 3.13 |
|---|