Moulin Fritte M70

Description: Monosilicate de Plomb

Oxide Analysis Formula Tolerance
PbO 78.80% 1.00
SiO2 21.20% 1.00
Oxide Weight 283.25
Formula Weight 283.25

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 455C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy