Description: SODA FELDSPAR

Oxide Analysis Formula Tolerance
CaO 2.32% 0.24
K2O 4.53% 0.27
Na2O 5.33% 0.49
Al2O3 18.01% 1.01
SiO2 69.81% 6.62
Oxide Weight 570.09
Formula Weight 570.09

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy