| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.45% | 2.10 | |
| Al2O3 | 0.39% | 1.00 | |
| P2O5 | 0.35% | 0.65 | |
| SiO2 | 98.71% | 429.56 | |
| Fe2O3 | 0.10% | 0.16 | |
| Oxide Weight | 26,153.85 | ||
| Formula Weight | 26,153.85 | ||
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |