Description: SODA FELDSPAR
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.05% | 0.10 | |
| K2O | 1.52% | 0.09 | |
| Na2O | 8.92% | 0.81 | |
| Al2O3 | 22.49% | 1.23 | |
| SiO2 | 66.03% | 6.15 | |
| Oxide Weight | 559.63 | ||
| Formula Weight | 559.63 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |