G.C. Powder

Description: ALPHA ALUMINA MONOHYDATE

Oxide Analysis Formula Tolerance
Na2O 0.01% -
Al2O3 70.00% 1.00
SiO2 0.02% -
Fe2O3 0.01% -
Oxide Weight 102.06
Formula Weight 102.06

Notes

Al2O3 is 70% minimum.

A special, high purity, alpha alumina monohydrate. It behaves like clay but desperses in an acid environment. Because of its high purity it leaves no deleterious fluxes in the grain boundaries after firing. It is an excellent plasticiser for conventional ceramic and refractory mixes. Its use will increase bulk density and improve high temperature thermal stability of the product.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy