Frit 34.410

Alternate Names: 34 410,34-410

Oxide Analysis Formula Tolerance
PbO 74.55% 1.00
Al2O3 4.77% 0.14
SiO2 20.68% 1.03
Oxide Weight 299.40
Formula Weight 299.40

Related Information

Data

Frit Melting Range (C) 900-1080C