1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 34.030

Alternate Names: Frit 34 030, Frit 34-030

Oxide Analysis Formula Tolerance
PbO 68.01% 0.94
K2O 1.22% 0.04 `
Na2O 0.40% 0.02
Al2O3 2.31% 0.07
SiO2 28.05% 1.44
Oxide Weight 308.51
Formula Weight 308.51

Related Information

Data

Frit Melting Range (C) 900-1080C