Chamosite

Description: High iron mineral

Oxide Analysis Formula Tolerance
SiO2 13.40% 1.17
Al2O3 7.40% 0.38
Fe2O3 8.50% 0.28
FeO 31.90% 2.05
MgO 2.50% 0.33
CaO 6.10% 0.57
P2O5 2.80% 0.10
H2O 8.50%n/a
CO2 17.40%n/a
Oxide Weight 381.10
Formula Weight 514.30