Geothite

Description: High iron mineral

Oxide Analysis Formula Tolerance
SiO2 5.40% 0.28
Al2O3 4.30% 0.13
Fe2O3 40.50% 0.79
FeO 8.70% 0.33
MnO 0.40% 0.02
MgO 1.60% 0.12
CaO 15.10% 0.84
TiO2 0.20% 0.01
P2O5 1.70% 0.04
H2O 7.20%n/a
CO2 15.00%n/a
Oxide Weight 242.80
Formula Weight 312.08