| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 53.00% | 3.08 | |
| Al2O3 | 30.00% | 1.03 | |
| Na2O | 4.50% | 0.25 | |
| CaO | 12.00% | 0.75 | |
| Oxide Weight | 347.31 | ||
| Formula Weight | 347.31 | ||
Analysis provided is of a sample material from Madagascar.