Sodalite

Description: A sodium aluminum silicate with chlorine

Formula: Na4Al3(SiO4)3Cl

Oxide Analysis Formula Tolerance
Al2O3 31.00% 0.75
Na2O 25.00% 1.00
SiO2 37.00% 1.53
Cl 7.00%n/a
Oxide Weight 230.64
Formula Weight 248.00