Siderite

Description: High iron mineral

Oxide Analysis Formula Tolerance
SiO2 7.80% 0.44
Al2O3 8.40% 0.28
Fe2O3 1.70% 0.04
FeO 35.60% 1.47
MnO 0.40% 0.02
MgO 4.00% 0.34
CaO 10.50% 0.63
TiO2 0.20% 0.01
P2O5 1.30% 0.03
H2O 4.20%n/a
CO2 25.30%n/a
Oxide Weight 236.48
Formula Weight 335.44