Trisodium Phosphate Hydrous

Alternate Names: T.S.P., TSP

Formula: Na3PO4.12H2O

Oxide Analysis Formula Tolerance
Na2O 24.47% 0.75
P2O5 18.68% 0.25
H2O 56.84%n/a
Oxide Weight 81.98
Formula Weight 189.95

Related Information

Links

URLs http://www.jcichem.com/jcipages/prodpgs/TrisodPho.html
Technical information on Trisodium Phosphate
Materials Trisodium Phosphate

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen