Description: AUSTRALIAN FELDSPAR
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.03 | |
| K2O | 10.30% | 0.62 | |
| MgO | 0.10% | 0.01 | |
| Na2O | 3.60% | 0.33 | |
| Al2O3 | 18.00% | 1.01 | |
| SiO2 | 67.00% | 6.36 | |
| Fe2O3 | 0.30% | 0.01 | |
| Oxide Weight | 568.38 | ||
| Formula Weight | 568.38 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |