Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Clay Body - Polar Ice
Foot Style - Flat unglazed
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 119 mm (4.7 in)
Weight - 385 grams (13.6 oz)