Serial Number: AJ50008
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed
Firing Schedule - C04PLTP
Temperature - Cone 04
Glaze Inside - G3879C
Glaze Outside - G3879C
Clay Body - L3924J
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 119 mm (4.7 in)
Height - 133 mm (5.2 in)
Weight - 366 grams (12.9 oz)
Not for sale