Honey glazed mug

Serial Number: AJ24382
Run/Test Number: P6973
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-B
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 118 mm (4.6 in)
Weight - 381 grams (13.4 oz)

Price:$0.00 (Not for sale, pieces being held for demo purposes)