Folded Polar Ice porcelain Sunshine mug
Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside (2483)
Folded Polar Ice porcelain Sunshine mug
Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside (2485)
Purple translucent Polar Ice porcelain mug
Thrown, incised, liner-glazed inside, dip-glazed outside (2495)
Matte red Polar Ice porcelain mug
Thrown, incised, liner-glazed inside, dip-glazed outside (2508)
Baby blue Polar Ice porcelain mug
Thrown, incised, liner-glazed inside, dip-glazed outside (2509)
Translucent Polar Ice porcelain mug
Thrown, incised, dip-glazed (2552)
Satin black folded M390 stoneware mug
Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside (2370)
Avail
Thrown, incised, liner-glazed inside, dip-glazed outside (2594)
Rutile blue buff MNS stoneware mug
Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table. (2373)
Matte red MNP porcelain mug
Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table. (2516)
Mugs made by Tony Hansen
2380 | 2378 | 2382 | 2385 | 2383 | 2386 | 2381 | 2379 | 2388 | 2466 | 2461 | 2470 | 2469 | 2452 | 2463 | 2455 | 2454 | 2460 | 2458 | 2465 | 2467 | 2457 | 2436 | 2437 | 2444 | 2447 | 2441 | 2448 | 2428 | 2340 | 2342 | 2358 | 2393 | 2397 | 2398 | 2400 | 2402 | 2403 | 2406 | 2416 | 2414 | 2409 | 2415 | 2411 | 2433 | 2422 | 2429 | 2431 | 2432 | 2361 | 2476 | 2477 | 2478 | 2489 | 2487 | 2490 | 2493 | 2488 | 2491 | 2479 | 2480 | 2474 | 2475 | 2350 | 2362 | 2367 | 2369 | 2355 | 2366 | 2345 | 2346 | 2352 | 2353 | 2394 | 2392 | 2391 | 2360 | 2343 | 2430 | 2453 | 2456 | 2462 | 2442 | 2446 | 2472 | 2471 | 2389 | 2505 | 2499 | 2510 | 2507 | 2511 | 2514 | 2504 | 2417 | 2376 | 2374 | 2375 | 2275 | 2549 | 2541 | 2537 | 2551 | 2538 | 2540 | 2539 | 2542 | 2543 | 2547 | 2546 | 2550 | 2545 | 2544 | 2533 | 2518 | 2531 | 2525 | 2527 | 2522 | 2529 | 2535 | 2556 | 2559 | 2562 | 2563 | 2565 | 2567 | 2568 | 2570 | 2571 | 2572 | 2574 | 2573 | 2558 | 2586 | 2585 | 2584 | 2583 | 2582 | 2588 | 2577 | 2576 | 2575 | 2591 | 2592 | 2587 | 2548 | 2368 | 2371 | 2532 | 2372 | 2520 | 2523 | 2405 | 2401 | 2459 | 2344 | 2341 | 2553 | 2561 | 2581 | 2580 | 2579 | 2578 | 2384 | 2348 | 2351 | 2390 | 2359 | 2339 | 2347 | 2404 | 2425 | 2424 | 2426 | 2427 | 2420 | 2419 | 2418 | 2281 | 2423 | 2421 | 2438 | 2443 | 2445 | 2440 | 2451 | 2481 | 2482 | 2484 | 2483 | 2485 | 2495 | 2508 | 2509 | 2552 | 2370 | 2594 | 2373 | 2516 | 2554 | 2502 | 2494 | 2410 | 2407 | 2408 | 2569 | 2557 | 2519 | 2357 | 2503 | 2530 | 2349 | 2289 | 2536 | 2560 | 2555 | 2521 | 2589 | 2515 | 2601 | 2603 | 2604 | 2605 | 2606 | 2607 | 2608 | 2609 | 2610 | 2611 | 2612 | 2613 | 2513 | 2614 | 2615 | 2616 | 2617 | 2618 | 2619 | 2620 | 2621 | 2622 | 2623 | 2624 | 2625 | 2626 | 2627 | 2628 | 2629 | 2630 | 2631 | 2632 | 2633 | 2634 | 2602 | 2635 | 2636 | 2637 | 2639 | 2640 | 2642 | 2643 | 2449 | 2399 | 2387 | 2354 | 2377
These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site.
My audience is potters, hobbyists and manufacturers.
Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made.
Since each has links into many areas of this site that provide more detail, researching just one mug could take hours!
The "AJxxxx" serial number on any can be searched here.