You won't find art language or "nice pot!" posts. It is about understanding, being serious about ware quality, saving energy, mixing your own, breaking the addiction to the trafficking in recipes, being independent.
This was made for our "AmacoGlazeLovers" Facebook group page (notice one fish is swimming the other way). Only three tile shapes are needed. The fish cutters were 3D printed to both cut and stamp at the same time. Multiple sizes of the triangle and trapezoid were made to accommodate irregularities and keep joints tighter. The clay is M340 and the glazes are Amaco Celadons and Potter's Choice (for brushing). I found the best way to paint them was to glue them down to a plaster slab with a few drops of glaze (it was easy to scrape off when the three coats had dried).