3DP | BSG | AIF | ABR | | BIN | ADV | AGT | PHY | ASR | uAz | ALM | ALS | E11 | JWK | ART | ARC | EBA | LAG | PBA | NFi | BLC | mQi | BIN | 62N | BIO | BSQ | CHP | BDT | BGD | BGP | BFR | Csu | DZc | BRK | HWi | SCS | MCB | SCB | ECS | CSP | OLC | CRE | CPM | CRS | STN | CST | LBS | TIL | C3D | CBM | CLM | ECM | CLO | SLR | CRT | CCT | CLT | GBG | CCO | CCN | CRP | d3S | CGS | OCS | DEC | DFT | TM2 | | Dux | DRP | DSP | ELE | ELT | MUE | SEU | EEE | MEQ | SCE | EQD | EQP | EQM | EMR | SER | EQS | | ETC | P3D | PAR | PAU | PCA | PBF | PDE | PGL | PKB | PMM | PPO | PPP | PSH | PWT | EXT | FEL | TAA | FRC | 9h6 | FLB | kK5 | FLS | FRT | MFM | YtL | F3D | EGK | GNM | DGE | GBC | GBS | GLS | GLI | GLC | GLM | GLR | GLT | MGL | FGE | GLZ | GEQ | EHE | HMT | h79 | HTR | CHS | Niv | I3D | ICS | IDP | IGR | EAP | ISO | Qno | qhK | KAO | KCD | EKB | KIL | MKL | SKL | LNS | LAB | vLv | FRL | 7hb | LEM | CQL | LTR | MSH | MOF | MAN | | MRK | MDS | MMC | MPC | MTS | MTT | | MAM | MAA | MDE | MTE | EMP | MPE | CLM | DEN | PWH | MAT | e38 | MTR | BDW | PMF | MIN | 3MM | MMK | EMM | MNC | EMF | yPu | NOX | SOC | | DSL | OPA | QKk | OXI | RED | PTT | SWS | PPS | PNC | PRP | | SPM | SPB | MPB | FRP | 9Hv | POI | PEN | PTW | PEQ | a87 | WKS | EPR | PRS | PRT | | PRD | PRO | | | | QCC | RMP | RSR | SRM | MRM | MGR | RFR | wWm | REF | SRS | EAR | ESK | SWR | | SCU | | YFh | SIL | ESR | LrD | YnJ | ESP | MSM | Tmx | STC | OLS | k67 | JXh | PWS | TWC | EPW | TCP | TCE | WSN | TLS | MTL | STL | TGR | OTR | | | UNI | UVR | FWK | gLF | WRS | WPS | YQd

Additives for Ceramic Glazes

Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.

Related Information

Links

Materials Ammonium Hydroxide
Materials CMC Gum
CMC gum is indispensable for many types of ceramic glazes. It is a glue and is mainly used to slow drying and improve adhesion and dry hardness.
Materials Colloid 211
Materials Epsom Salts
Employed in ceramics as a flocculant to thicken and gel suspensions by electrostatically charging particles so that they attract each other.
Materials Ethylamine
Materials Gum Arabic
Materials Methocel
Materials Sodium Hydroxide
Materials Sodium Oxalate
Materials Sodium Phosphate
Materials Sodium Polyacrylate
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.
Materials Acti-Gel 208
Materials Peptapon
Materials Constrabind NS-1001 V i
Materials Tetrasodium Pyrophosphate
Materials Tetrasodium Pyrophosphate Hydrated
Materials Sodium Hexametaphosphate
Materials Garamite
Materials Claytone
Materials Calcium Chloride
Commonly used as a flocculating agent in ceramic glazes (to suspend and gel them).
Materials Copper Sulfate
Materials Mormate
Materials Rhodopol
Materials Optapix
Materials Methylcellulose
Materials Xantham Gum
Materials Mineral Colloid BP
Materials Vanzan
Materials Sodium Silicate
A sticky, viscous liquid. The most common deflocculant used in ceramics. Also used as a bonding agent.
Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Glossary Ceramic Binder
Binders are glues that harden ceramic powders as they dry. They enable improved surface adherence. And slower drying.
Glossary Ceramic Glaze
Ceramic glazes are glasses that have been adjusted to work on and with the clay body they are applied to.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy