50-250C | 80C-250C | 120C | 150C | 180C | 185C | 200C | 200C-1000C | 200C-450C | 210C-280C | 250C-370C | 260C | 290C | 300C-330C | 300C | 370-950C | | 400C | 425C-650C | 480C-600C | 500C-600C | 512C | 535C | 540C-600C | 650C-900C | 700F | 750C-1000C | 750-850 | 800C-1100C | 850-950 | 850C | 850C+ | 900-1000 | 900C | 990C | 1025-1325 | 1025C+ | 1050C | 1050C | 1082C | 1100C+ | 1100C | 1100C | 1300C | 1325C | 1330C | 1360C | 1400F | 1400F | 1418C-1428C | 1420C | 1500F | 1550C | 1565C | 1600F-1650F | 1650F | 1785C | 1800F | 1950F-2050F | 1990C | 2300C | 2320C | 2750F

400C-600C

Dehydroxylation of Kaolin

After free moisture is removed during the calcination of raw kaolin, chemically bound water is driven off producing metakaolin.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy