AO | B1 | CE | F5 | F5-3NO-E1 | FO | G1214M | G1214W | G1214Z | G1215U | G1216L | G1216M | G1916Q | G1947U | G2000 | G2240 | G2571A | G2587 | G2826X | g2851H | G2853B | G2896 | G2902B | G2902D | G2916F | G2926B | G2926J | G2926S | G2928C | G2931H | G2931K | G2931L | G2934 | G2934Y | G3806C | G3838A | G3879 | GA10-A | GA10-B | GA10-D | GA10x-A | GA6-A | GA6-AR | GA6-B | GA6-C | GA6-D | GA6-F | GA6-G | GA6-G1 | GA6-H | GBCG1 | GBCG2 | GC | GR | GR10-A | GR10-B | GR10-C | GR10-E | GR10-G | GR10-J | GR10-J1 | GR10-K1 | GR10-L | GR6-A | GR6-B | GR6-C | GR6-D | GR6-E | GR6-H | GR6-L | GR6-M | GR6-N | L2000 | L3341B | L3500E | L3617A | L3685U | L3724F | L3924C | L3954B | L3954N | P3998 | P5283 | TF | | WM | ZZ1

VS - Vesuvius Fara Shimbo Crystalline Glaze

Modified: 2009-05-23 11:14:46

Titanium-Free Crystalline Glaze

Material Amount
Ferro Frit 311050.00
Zinc Oxide25.00
Silica18.00
Whiting5.00
Magnesium Carbonate2.00
100.00

Notes

Matures at cone 9. Completely transparent ground and easily grown crystals very white when no other colorants are used. Surface is relatively hard and very glossy. Crystals often have a central "peak."

Related Information

Links

Firing Schedules Shimbo Crystal Schedule 1
Typecodes Crystalline Glaze Recipe Fara Shimbo
These are from Fara\'s Crystal Glazes book II.

XML to Paste Into Desktop Insight

<recipes>XML not functional: We are working on this problem.</recipes>

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture

Please check recaptcha to proceed


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved