AO | B1 | CE | F5 | | FO | G1214M | G1214W | G1214Z | G1215U | G1216L | G1216M | G1916Q | G1947U | G2000 | G2240 | G2571A | G2587 | G2826X | g2851H | G2853B | G2896 | G2902B | G2902D | G2916F | G2926B | G2926J | G2926S | G2928C | G2931H | G2931K | G2931L | G2934 | G2934Y | G3806C | G3838A | G3879 | GA10-A | GA10-B | GA10-D | GA10x-A | GA6-A | GA6-AR | GA6-B | GA6-C | GA6-D | GA6-F | GA6-G | GA6-G1 | GA6-H | GBCG1 | GBCG2 | GC | GR | GR10-A | GR10-B | GR10-C | GR10-E | GR10-G | GR10-J | GR10-J1 | GR10-K1 | GR10-L | GR6-A | GR6-B | GR6-C | GR6-D | GR6-E | GR6-H | GR6-L | GR6-M | GR6-N | L2000 | L3341B | L3500E | L3617A | L3685U | L3724F | L3924C | L3954B | L3954N | P3998 | P5283 | TF | VS | WM | ZZ1

F5-3NO-E1 - Fa's Blue Heaven Fara Shimbo Crystalline

Modified: 2009-05-23 11:16:32

Nickel teal crystals on a transparent amber ground

Material Amount Percent
Ferro 311050.00
Zinc Oxide27.00
Silica14.00
Spodumene5.00
Dolomite4.00
Titanium Dioxide2.00
Nickel Oxide3.00
105.00

Notes

This is so far the best base from which to obtain true nickel teal crystals (caused by nickel zinc silicate) on an amber ground (caused by nickel spinels). The glaze should be used within a day of being mixed for best results. It will take a lower firing but this will almost ensure the formation of hatrurite (calcium silicate) crystals so numerous that the blue zinc crystals have nowhere to grow.

Related Information

Links

Firing Schedules Shimbo Crystal Schedule 1
Typecodes Crystalline Glaze Recipe Fara Shimbo
These are from Fara\'s Crystal Glazes book II.

XML to Paste Into Desktop Insight

<recipes>XML not functional: We are working on this problem.</recipes>

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy