By preparing these three tests you can measure many properties of a clay body. These include drying shrinkage, fired shrinkage, porosity, drying performance, soluble salts content, water content and LOI.
Tests | Drying Factor |
---|---|
Tests | Shrinkage/Absorption Test |
Glossary |
Drying Performance
In ceramics, drying performance is very important to optimizing production. More plastic clays shrink more and crack more, but they are also better to work with. |
Glossary |
Physical Testing
In ceramics, glazes and bodies have a chemistry, a mineralogy and a physical presence. All of these need to be understood to adjust and fix issues. |
Glossary |
LOI
Loss on Ignition is a number that appears on the data sheets of ceramic materials. It refers to the amount of weight the material loses as it decomposes to release water vapor and various gases during firing. |