On the right is the G2934Y matte base recipe with only 8% Cerdec Orange encapsulated stain. G2934Y employs a frit-source for the MgO (as opposed to G2934 which sources the MgO from dolomite). If this was a glossy glaze the required percentage of stain would be higher. Other colors (like yellow, red, blue, black), are equally vibrant. But not all (e.g. purple), testing is needed. The porcelain is Plainsman Polar Ice.
Recipes |
G2934 - Matte Glaze Base for Cone 6
A base MgO matte glaze recipe fires to a hard utilitarian surface and has very good working properties. Blend in the glossy if it is too matte. |
---|---|
Recipes |
G2934Y - Cone 6 Magnesia Matte Low LOI Version
The same chemistry as the widely used G2934 but the MgO is sourced from a frit and talc instead of dolomite. It has a finer surface, less cutlery marking and staining. |
Glossary |
Encapsulated Stain
This is a type of stain manufacture that enables the use of metal oxides (like cadmium) under temperature conditions in which they would normally fail. |
Glossary |
Matte Glaze
Random material mixes that melt well overwhelmingly want to be glossy, creating a matte glaze that is also functional is not an easy task. |
Articles |
Concentrate on One Good Glaze
It is better to understand and have control of one good base glaze than be at the mercy of dozens of imported recipes that do not work. There is a lot more to being a good glaze than fired appearance. |