I counter-balanced the measuring cup and weighed out 250g of water. Then I added 100g of Laguna gum solution and stirred it. I put that into the blender and added 500g of powdered glaze (you can use any glaze recipe). I started the blender on slow then increased it one-at-a-time to full speed. After less than a minute (and a little work with a spatula) it was creamy smooth. It painted evenly on the tile just like a commercial bottled glaze, drying slowly. This produces a specific gravity of 1.58 (which is pretty high) so I can add water and thin it with no issues.