The flow on the left is an adjusted Perkins Frit Clear (we substituted frit for Gerstley Borate). It is a cone 6 transparent that appeared to work well. However it did not survive a 300F oven-to-icewater IWCT test without crazing on Plainsman M370. The amount of flow (which increases a little in the frit version) indicates that it is plenty fluid enough to accept some silica. So we added 10% (that is the flow on the right). Now it survives the thermal shock test and still fires absolutely crystal clear.
Recipes |
G2926B - Cone 6 Whiteware/Porcelain Transparent Base Glaze
A base transparent glaze recipe created by Tony Hansen for Plainsman Clays, it fires high gloss and ultra clear with low melt mobility. |
---|---|
Media |
How I Improved a Popular Cone 6 Clear Glaze Using Insight-Live
How I found a ceramic glaze recipe on Facebook, substituted a frit for the Gerstley Borate, added the extra SiO2 it needed and got a fabulous more durable cone 6 clear. |
Oxides | MgO - Magnesium Oxide, Magnesia |
Oxides | SiO2 - Silicon Dioxide, Silica |