Description: High iron mineral
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 5.40% | 0.28 | |
| Al2O3 | 4.30% | 0.13 | |
| Fe2O3 | 40.50% | 0.79 | |
| FeO | 8.70% | 0.33 | |
| MnO | 0.40% | 0.02 | |
| MgO | 1.60% | 0.12 | |
| CaO | 15.10% | 0.84 | |
| TiO2 | 0.20% | 0.01 | |
| P2O5 | 1.70% | 0.04 | |
| H2O | 7.20% | n/a | |
| CO2 | 15.00% | n/a | |
| Oxide Weight | 242.80 | ||
| Formula Weight | 312.08 | ||