Oxide Analysis Formula
PbO 65.00% 1.00
Al2O3 3.00% 0.10
SiO2 32.00% 1.83
Oxide Weight 343.38
Formula Weight 343.38

Notes

Sub: Ferro 3602
Raw color: Very light yellow
Form: Granular or finely ground frit
Specific Gravity: 4.6
Density, lbs/cu ft, Granlar: 155-175; Ground: 135-155
Melting Range: 788-816C

Sieve Analysis: Granular Ground
+7 mesh 0 +100 mesh 1.0%
+10 mesh 1.3% +200 mesh 1.2%
+20 mesh 81.3% +325 mesh 7.8%
+40 mesh 10.0%
+80 mesh 2.6%

CAS Number: 65-997-18-4

Related Information

Links

Materials Frit
Materials Ceraflux
Materials Ferro Frit 3489
Materials BPS Lead Bisilicate
Materials Lead Bisilcate B-15
Materials Lead Bisilicate Frit
Materials Ferro Frit 3626
Materials Frit 3647
Typecodes Frit
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

Data

Frit Softening Point800C
Frit Softening Point788-816C
Density (Specific Gravity)4.50
Density (Specific Gravity)4.55-4.7

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy