Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3498

Alternate Names: F3498

Description: Lead alumina bisilicate

Oxide Analysis Formula Tolerance
PbO 65.30% 1.00
Al2O3 2.50% 0.08
SiO2 32.20% 1.83
Oxide Weight 341.81
Formula Weight 341.81

Related Information

Links

Materials Ferro Frit 3602
A lead bisilicate frit with 2.5% alumina oxide.
Materials Ferro Frit 4064
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Ferro Frit CE VTR 29
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 815C M
Density (Specific Gravity) 4.50

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.