Ajax Glomax Kaolin

Oxide Analysis Formula
CaO 0.26% 0.01
K2O 0.06% 0.00
MgO 0.30% 0.02
Na2O 0.02% 0.00
TiO2 1.54% 0.05
Al2O3 38.71% 1.00
SiO2 45.94% 2.01
Fe2O3 0.45% 0.01
LOI12.71%
Oxide Weight 229.98
Formula Weight 263.47

Related Information

Links

Materials Kaolin
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.