Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Arsenic Oxide | Asbestos: A Difficult-to-Repace Material | Ball Clay | BARIUM and COMPOUNDS / Toxicology | Barium Carbonate | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Kaolin Toxicity | Lead Chromate | Lead in Ceramic Glazes: What Did We Learn? | Lead in Frits: The Hazards | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | The Use of Barium in Clay Bodies | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Asbestos: A Difficult-to-Repace Material

Asbestos is not used in ceramic body or glaze formulations, it is used to make insulating boards and blankets for kilns and furnaces. It performs extremely well as a refractory and has been difficult to replace, it is still used. A number of man-made fibers have been developed but these have presented similar health hazards and have proven unsuitable for other reasons. Soluble fibers have been introduced, these dissolve over time in the lungs. However they are not as refractory.

Asbestos is a fibrous magnesium silicate. Its hazards are well known and related to the particle shape and size and the ease with which these can be trapped deep within the air pockets of the lungs. Companies that used or use asbestos have been mandated to create websites to manage legal claims against them, especially by their workers. Talc is also a fibrous magnesium silicate.

Related Information

Links

Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?
Hazards Talc Toxicology
Hazards Man-Made Vitreous Fibers (MMVF) Toxicology
Satety and hazard info of aluminum silicate ceramic fiber materials (e.g. fibre glass, mineral wood, refractory ceramic fibre).
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc00/icsc0014.htm
Asbestos at ilo.org
URLs https://www.asbestos.com/companies/a-p-green-industries.php
AP Green Asbestos Use
Minerals Asbestos

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy