0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Co-efficient of Thermal Expansion | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Substitution | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once fire glazing | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silica:Alumina Ratio | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Salt firing

Salt firing is a process where unglazed ware is fired to high temperatures and salt is introduced to produce a vapor that glazes the ware.

Key phrases linking here: salt glazing, salt-glazing, salt firing, soda firing, salt fired, salt-fired - Learn more

Details

Salt firing is a process where unglazed ware is fired to high temperatures and salt fumes are introduced into the kiln chamber (normally by a spray in the burner ports). The sodium in the salt forms a vapour cloud in the kiln. That sodium, along with the silica and alumina in the clay, combine to form a glass to glaze the ware. Bodies that contain high silica thus form the best interface with the glaze.

The salt glazing process has many historical roots. Salt glazed ware typically has distinctive marbled and variegated surface effects. Many books showcase these. An increasing number of web pages extol the process and potters pay considerable amounts to attend workshops to learn about it. There is, however, a bias toward describing the process in the language of art rather than science. One potter described her preference for the process saying that "the voice of the fire just does not speak to her" in electric-fired ware, with soda firing her ware "says what she wants it to say". And the historic and cultural biases, rather than logic, tend to push the methods and processes used.

Salt glazed ware can be suitable for functional use, but there are caveats. Sodium has the highest thermal example of all common oxides so glazes are almost certain to craze. This will greatly impact ware strength and functionality. Not surprisingly, the oxide formulas of salt glazes fall well outside of normal glaze chemistry profiles. That means there is a danger of surface leaching, resulting in a loss of gloss or change in appearance. It is thus desirable to use a fitted liner glaze on functional pieces. Sodium is a very active flux and the salt-glazing process is theoretically feasible at lower temperatures than are commonly done. Whatever the range used, the body should be vitreous to produce strong ware.

Sodium vapor glazing using compounds other than sodium chloride (table salt) is practiced by many people.

There has been quite a bit of discussion about the safety and environmental concerns of salt vs. soda firing. It does not appear to be a foregone conclusion that soda is better than salt or even that chlorine is released in salt firings (rather than HCL vapor). Some reports on the Internet claim that measurements done on kilns have demonstrated that salt firing is as clean or cleaner than fuel reduction firing.

Related Information

Salt glazed pieces often craze


This picture has its own page with more detail, click here to see it.

Crazing in glazes is common in this type of ware but since the body is fired well into vitrification this is not considered a problem (the unique aesthetics of this type of ware trump such issues). Salt glazes, by their very nature, are high in sodium. Since Na2O has such high thermal expansion pieces are almost guaranteed to craze. This was from kiln at the Medalta artist in residence program

Wood/Soda fired Cone 10 mug by John Cummings


This picture has its own page with more detail, click here to see it.

A salt glazed sewer pipe junction


A salt glazed sewer pipe junction

This picture has its own page with more detail, click here to see it.

Made at Alberta Clay Products in Alberta, Canada about 1960. These are massive. They were hand-constructed. This was fired in a beehive kiln and is on display inside one next to the Plainsman Clays plant (a historic site). Ceramic glazes are normally slurries of clay, quartz and and fluxes like sodium feldspar, calcium carbonate or dolomite - these are applied to ware before firing. But, in this salt-glazing process, common table salt was literally shovelled into a hole at the top as the kiln reached temperature (about 2350F)! The salt decomposed, separating into sodium vapour and chlorine gas within the chamber and the sodium reacted with the quartz-containing clay to form a durable glaze. Unfortunately the chlorine gas escaped into the air!

Plainsman P580, P600, H570 soda fired samples


This picture has its own page with more detail, click here to see it.

These fire ivory to bone with in reduction.

Soda and salt kilns at the Medalta International Artists in Residence


This picture has its own page with more detail, click here to see it.

In Medicine Hat, Alberta, Canada. Designed by Aaron Nelson.

Rear of soda and salt kilns at the Medalta International Artists in Residence


This picture has its own page with more detail, click here to see it.

In Medicine Hat, Alberta, Canada. Designed by Aaron Nelson.

Salt glaze beehive kiln beside the Plainsman Clays plant


This picture has its own page with more detail, click here to see it.

This was built just after the turn of the 20th century and was one of about 20 at the Alberta Clay Products company. It was used to fire salt-glazed ceramic pipe, these were used for municipal sewer and water lines. A ceramic industry quickly grew in the city because it had good clay, natural gas, plenty of water, a dry climate, industrious people, a large river and it was on the Trans Canada highway and railway.

A studio salt kiln being unloaded


This picture has its own page with more detail, click here to see it.

Notice how ware is set on pads of clay to enable the salt vapours to access the underside. Salt and soda kilns degrade over time as the sodium eats away at the interior bricks. Shelves must be covered in kiln wash to preserve them.

Links

Glossary Kiln Firing
All types of ceramic are fired in a kiln to cement particles together to produce a hard and water and temperature resistant product.
Glossary Flashing
A visual effect that occurs in wood and salt firing of ceramic ware. Many potters value the effect and use special materials and firing methods to enhance it.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy